Ferropericlase

(Mg0.9375Fe0.0625)O

third-order Birch-Murnaghan · Original · 2020

Why this differs from similar rows?

Table I value for the mixed-spin (MS: one HS and one LS Fe) state with iron ions modeled as 11th neighbors (11nn); sibling rows cover HS/LS states and the 2nn configuration.

V₀
73.86
ų
Unit cell
K₀
171.300
GPa
Unknown
K′
4.230
dimensionless

Volume (V₀)

Value Unit Basis Z
73.86 ų Unit cell

Reported value and unit are preserved as extracted. Z (formula units per cell) is not stored yet, so molar ↔ ų/f.u. conversion is not applied automatically.

Composition

OxideMolar
MgO0.9375
FeO0.0625

Formula: (Mg0.9375Fe0.0625)O

Conditions & method

Tref
Pref
Structure
B1 rocksalt (Fm-3m)
Method
DFT+U / DFT+DMFT
static ab initio DFT LSDA+Usc calculation
Sample
6Fp, 11nn Fe configuration, MS state (1HS and 1LS)

Source

Paper
Phonon dispersion throughout the iron spin crossover in ferropericlase
Authors
Michel L. Marcondes; Fawei Zheng; Renata M. Wentzcovitch
DOI
10.1103/physrevb.102.104112
Year
2020
Journal
Physical review. B./Physical review. B
Origin
Original (measured or fitted in the source paper)

Evidence from the paper

TABLE I. Equation of state parameters obtained in static LSDA +Usc calculations in Fp. XFe 0.0625 (11nn), MS (1HS and 1LS): V0 (Å3) 73.86, K0 (GPa) 171.3, K0' 4.23.

Additional notes

conditions
static (0 K) calculation
spin state
mixed spin (MS: one HS and one LS iron)
iron configuration
iron ions as 11th neighbors (11nn)