← Browse · Ferropericlase

Ferropericlase

(Mg0.9375Fe0.0625)O

third-order Birch-Murnaghan · Original · 2020

Why this differs from similar rows?

Table I value for the low-spin (LS) state with iron ions modeled as 11th neighbors (11nn); sibling rows cover HS/MS spin states and the 2nn configuration.

V₀
73.32
ų
Unit cell
K₀
174.800
GPa
Unknown
K′
4.170
dimensionless

Volume (V₀)

Value Unit Basis Z
73.32 ų Unit cell

Reported value and unit are preserved as extracted. Z (formula units per cell) is not stored yet, so molar ↔ ų/f.u. conversion is not applied automatically.

Composition

OxideMolar
MgO0.9375
FeO0.0625

Formula: (Mg0.9375Fe0.0625)O

Conditions & method

Tref
Pref
Structure
B1 rocksalt (Fm-3m)
Method
DFT+U / DFT+DMFT
static ab initio DFT LSDA+Usc calculation
Sample
6Fp, 11nn Fe configuration, LS state

Source

Paper
Phonon dispersion throughout the iron spin crossover in ferropericlase
Authors
Michel L. Marcondes; Fawei Zheng; Renata M. Wentzcovitch
DOI
10.1103/physrevb.102.104112
Year
2020
Journal
Physical review. B./Physical review. B
Origin
Original (measured or fitted in the source paper)

Evidence from the paper

TABLE I. Equation of state parameters obtained in static LSDA +Usc calculations in Fp. XFe 0.0625 (11nn), LS: V0 (Å3) 73.32, K0 (GPa) 174.8, K0' 4.17.

Additional notes

conditions
static (0 K) calculation
spin state
low spin (LS)
iron configuration
iron ions as 11th neighbors (11nn)