← Browse · Periclase

Periclase

MgO

none (not an EOS fit) · Cited · 2000

Why this differs from similar rows?

Table 2 cites Ref. 8 (Jackson & Niesler), ultrasonic measurements to only 3 GPa; sibling row cites a different study (Ref. 14) measured to 37 GPa.

V₀
Unknown basis
K₀
162.500
GPa
Adiabatic
K′
4.130
dimensionless

Volume (V₀)

Value Unit Basis Z
Unknown basis

Reported value and unit are preserved as extracted. Z (formula units per cell) is not stored yet, so molar ↔ ų/f.u. conversion is not applied automatically.

Composition

OxideMolar
MgO1

Formula: MgO

Conditions & method

Tref
Pref
Structure
B1 rocksalt (Fm-3m)
Method
experiment (Brillouin / ultrasonic / elasticity)
ultrasonic measurements (0–3 GPa), literature value
Sample
single-crystal MgO, ultrasonic (Jackson and Niesler, Ref. 8)

Source

Paper
Elasticity of MgO and a primary pressure scale to 55 GPa
Authors
Chang‐Sheng Zha; Ho‐kwang Mao; Russell J. Hemley
DOI
10.1073/pnas.240466697
Year
2000
Journal
Proceedings of the National Academy of Sciences
Origin
Cited (quoted from earlier work)

Evidence from the paper

Table 2: Ref. 8† (0–3 GPa): K0S = 162.5(2) GPa, K'0S = 4.13(9), K''0S = -0.058(66) GPa^-1. '†Elastic moduli were fit to the polynomial Mij(P) = Mij0 + M'ij0 P + 0.5 M''ij0 P^2.'

Additional notes

Kpp0S per GPa
-0.058(66)
reference
Jackson & Niesler (1982)