← Browse · Post-perovskite

Post-perovskite

MgSiO3

Keane · Original · 2016

Why this differs from similar rows?

'fit6': same dataset as fit5 but with V0 and K-infinity' fixed to the fit5 values (157.16, 2.19) while other parameters are refit; V0/K0/K' match fit5 but theta0/beta differ.

V₀
157.16
ų/cell
Formula unit
K₀
310
GPa
Isothermal
K′
3.470
dimensionless

Volume (V₀)

Value Unit Basis Z
157.16 ų/cell Formula unit

Reported value and unit are preserved as extracted. Z (formula units per cell) is not stored yet, so molar ↔ ų/f.u. conversion is not applied automatically.

Composition

OxideMolar
MgO1
SiO21

Formula: MgSiO3

Conditions & method

Tref
300 K
Pref
Structure
post-perovskite (CaIrO3-type, Cmcm)
Method
experiment (XRD / DAC / multianvil compression)
LHDAC powder X-ray diffraction
Sample
fit6 (This study + Guignot et al. data, V0 and K∞′ fixed to fit5 values)

Source

Paper
Experimental and theoretical thermal equations of state of MgSiO3 post-perovski…
Authors
Takeshi Sakai; Haruhiko Dekura; Naohisa Hirao
DOI
10.1038/srep22652
Year
2016
Journal
Scientific Reports
Origin
Original (measured or fitted in the source paper)

Evidence from the paper

Table 1: 157.16 fix | 310± 2 | 3.47± 0.05 | γ0=1.44± 0.09 | γ∞=0.93 fix | β=2.8± 0.3 | θ0=938± 240 | K∞′=2.19 fix | fit6 | Exp., LHDAC | T-MgO(Keane)

Additional notes

fit number
fit6
gamma0
1.44± 0.09
gamma inf
0.93 fix
beta
2.8± 0.3
theta0 K
938± 240
K inf prime
2.19 fix
pressure scale
T-MgO(Keane): Tange et al. MgO scale