← Browse · Stishovite

Stishovite

SiO2

unknown · Cited · 2020

Why this differs from similar rows?

Cites literature static DAC data (ref. 5), K0=309.9 GPa, K0'=4.59; other rows cite different original references.

V₀
Unknown basis
K₀
309.900
GPa
Unknown
K′
4.590
dimensionless

Volume (V₀)

Value Unit Basis Z
Unknown basis

Reported value and unit are preserved as extracted. Z (formula units per cell) is not stored yet, so molar ↔ ų/f.u. conversion is not applied automatically.

Composition

OxideMolar
SiO21

Formula: SiO2

Conditions & method

Tref
Pref
Structure
rutile-type (stishovite)
Method
experiment (XRD / DAC / multianvil compression)
static diamond anvil cell compression (literature)
Sample
literature static DAC data (ref 5)

Source

Paper
Evidence of shock-compressed stishovite above 300 GPa
Authors
M. Schoelmerich; T. Tschentscher; Shrikant Bhat; C. A. Bolme; Eric Cunningham; Robert Farla; Eric Galtier; A. E. Gleason; M. Harmand; Yuichi Inubushi; Kento Katagiri; Kohei Miyanishi; Bob Nagler; Norimasa Ozaki; Thomas R. Preston; R. Redmer; Ray F. Smith; Tsubasa Tobase; Tadashi Togashi; S. J. Tracy; Y. Umeda; L. Wollenweber; T. Yabuuchi; U. Zastrau; Karen Appel
DOI
10.1038/s41598-020-66340-y
Year
2020
Journal
Scientific Reports
Origin
Cited (quoted from earlier work)

Evidence from the paper

as well as EOS studies of stishovite at lower pressures from static DAC experiments (K0 = 309.9 GPa, K0' = 4.59 GPa5; ...)

Additional notes

reference
citation 5
note Kp unit
Paper writes 'GPa' after K0' verbatim