Stishovite
SiO2
unknown · Cited · 2024
Why this differs from similar rows?
Table cites Yang and Wu (2014), theoretical calculation re-fit to 15 GPa/727 C; other rows cite different original studies/methods.
V₀
—
Unknown basis
K₀
290.100
GPa
Adiabatic
K′
5.020
dimensionless
Volume (V₀)
| Value | Unit | Basis | Z |
|---|---|---|---|
| — | — | Unknown basis | — |
Reported value and unit are preserved as extracted. Z (formula units per cell) is not stored yet, so molar ↔ ų/f.u. conversion is not applied automatically.
Composition
| Oxide | Molar |
|---|---|
| SiO2 | 1 |
Formula: SiO2
Conditions & method
- Tref
- —
- Pref
- —
- Structure
- —
- Method
- first-principles DFT / ab initioTheoretical calculation (DFT, local density approximation)
- Sample
- —
Source
- Paper
- Sound Velocities of Stishovite at Simultaneous High Pressure and High Temperatu…
- Authors
- Sibo Chen; Siheng Wang; Xintong Qi; Man Xu; Tony Yu; Yanbin Wang; Baosheng Li
- DOI
- 10.1029/2023gl107700
- Year
- 2024
- Journal
- Geophysical Research Letters
- Origin
- Cited (quoted from earlier work)
Evidence from the paper
Table 1 (Yang and Wu (2014), Theoretical calculation): K_S0 = 290.1 GPa, K_S' = 5.02, dKS/dT = -0.027 GPa/K, G0 = 213.1 GPa, G' = 1.71, dG/dT = -0.018 GPa/K, Pmax = Re-fit to 15.0, Tmax = Re-fit to 727.
Additional notes
reference
Yang and Wu (2014)
dKS dT
-0.027 GPa/K
G0
213.1 GPa
G prime
1.71
dG dT
-0.018 GPa/K
P max
Re-fit to 15.0 GPa
T max
Re-fit to 727 degC