← Browse · Corundum

Corundum

Al2O3

third-order Birch-Murnaghan · Original · 2022

Why this differs from similar rows?

Table 2 Model 2 with theta_D0 fixed to 800 K; sibling rows fix theta_D0 to different values (500 K, 1,100 K), changing the fitted K_T0.

V₀
255.1
ų
Unit cell
K₀
245
GPa
Isothermal
K′
4
dimensionless

Volume (V₀)

Value Unit Basis Z
255.1 ų Unit cell

Reported value and unit are preserved as extracted. Z (formula units per cell) is not stored yet, so molar ↔ ų/f.u. conversion is not applied automatically.

Composition

OxideMolar
Al2O31

Formula: Al2O3

Conditions & method

Tref
300 K
Pref
Structure
corundum
Method
experiment (XRD / DAC / multianvil compression)
synchrotron X-ray diffraction in laser-heated diamond anvil cells, Pt/NaCl pressure calibrants
Sample
Table 2, Model 2 (θD0 = 800 K fixed)

Source

Paper
Thermal Equations of State of Corundum and Rh2O3 (II)‐Type Al2O3 up to 153 GPa …
Authors
Weigang Shi; Wei Wei; Ningyu Sun; Zhu Mao; Vitali B. Prakapenka
DOI
10.1029/2021jb023805
Year
2022
Journal
Journal of Geophysical Research Solid Earth
Origin
Original (measured or fitted in the source paper)

Evidence from the paper

Table 2 (Thermoelastic Parameters of Corundum With Varying θD0), Model 2: KT0 = 245(1) GPa, KT0' = 4(fixed), V0 = 255.1(fixed) Å3, θD0 = 800(fixed) K, γ0 = 1.26(6), q = 0.7(3).

Additional notes

theta D0 K
800(fixed)
gamma 0
1.26(6)
q
0.7(3)