← Browse · Stishovite

Stishovite

pure SiO2 (0 wt% Al2O3, 0 wt% H2O)

none (not an EOS fit) · Cited · 2007

V₀
Unknown basis
K₀
316
GPa
Adiabatic
K′
dimensionless

Volume (V₀)

Value Unit Basis Z
Unknown basis

Reported value and unit are preserved as extracted. Z (formula units per cell) is not stored yet, so molar ↔ ų/f.u. conversion is not applied automatically.

Composition

OxideMolar
SiO21

Formula: pure SiO2 (0 wt% Al2O3, 0 wt% H2O)

Conditions & method

Tref
Pref
Structure
rutile-type (stishovite)
Method
experiment (Brillouin / ultrasonic / elasticity)
Brillouin scattering (literature values, Weidner et al. 1982)
Sample
pure stishovite (Weidner et al. 1982)

Source

Paper
Effect of Al3+ and H+ on the elastic properties of stishovite
Authors
D. L. Lakshtanov; Konstantin D. Litasov; Stanislav Sinogeikin; H. Hellwig; Jie Li; Eiji Ohtani; Jay D. Bass
DOI
10.2138/am.2007.2294
Year
2007
Journal
American Mineralogist
Origin
Cited (quoted from earlier work)

Evidence from the paper

Table 4. Aggregate elastic moduli for K324 and K325 compared to pure stishovite data (Weidner et al. 1982): Ks (GPa) 316(4); KT (GPa) 312(4); Gs (GPa) 220(3); rho (g/cm3) 4.29.

Additional notes

KT GPa
312(4)
G S GPa
220(3)
density g cm3
4.29
vp
11.923(30)
vs
7.165(30)
reference
Weidner et al. 1982