post-aragonite CaCO3-Pmmn

CaCO3

third-order Birch-Murnaghan · Cited · 2020

Why this differs from similar rows?

Table 1 row re-analyzing Ono et al. (2005) data (NaCl medium) under the Pt pressure scale of Fei et al. (2007), K' fixed to 4; sibling row re-analyzes Lobanov et al. (2017) data.

V₀
99.4
ų
Unit cell
K₀
118
GPa
Isothermal
K′
4
dimensionless

Volume (V₀)

Value Unit Basis Z
99.4 ų Unit cell

Reported value and unit are preserved as extracted. Z (formula units per cell) is not stored yet, so molar ↔ ų/f.u. conversion is not applied automatically.

Composition

OxideMolar
CaO1
CO21

Formula: CaCO3

Conditions & method

Tref
300 K
Pref
Structure
other / unspecified
Method
experiment (XRD / DAC / multianvil compression)
XRD (PM: NaCl)
Sample
Ono et al. (2005), refitted by Pt pressure scale (Fei et al. 2007) (Table 1)

Source

Paper
Thermal equation of state of post-aragonite CaCO3-Pmmn
Authors
Mingda Lv; Jiachao Liu; Eran Greenberg; Vitali B. Prakapenka; Susannah M. Dorfman
DOI
10.2138/am-2020-7279
Year
2020
Journal
American Mineralogist
Origin
Cited (quoted from earlier work)

Evidence from the paper

Table 1: 99.4(20) | 118(14) | 4 (fixed) | XRD (PM: NaCl) | Ono et al. (2005), Refitted by the pressure scale of Pt (Fei et al. 2007).